Our mainly stainless steel grade: ASTM/ASME Grade 304, Grade 304L,304h, 316, 316L, 316H, 316TI, 321, 321H, 309S, 309H, 310S, 310H, 410S, 2205, 904L, 2507, 254, gh3030, 625, 253MA, S30815, 317L, Type 317, 316lN, 8020, 800, 800H, C276, S32304 and others special requirement stainless steel grade.
Stainless Steel
- Fusion welding efficiency for type 304 stainless steel is great both with and without fillers.
- 304L can, therefore, be used “as welded” in extreme corrosion environments, and it eliminates the necessity for annealing.
- Recommended filler rods and electrodes for stainless-steel 304 is grade 308 chrome steel.
Grade 304L is extra resistant to carbide precipitation and could be heated into the above temperature vary. Continuous use of 304 within the °F vary is not recommended if subsequent aqueous corrosion resistance is important.